Fundamentals

The atomic structure

The atomic model

An atom is the smallest chemically not further divisible component of matter. Depending on the atom, it is composed of a certain number of electrons, protons, and neutrons. The positively charged protons and the neutrons form the nucleus, which is encircled by the electrons in certain intervals. A naturally occurring atom is electrically neutral, there are just as many positive protons as negatively charged electrons inside an atom. While the number of neutrons can vary. The simplest atom is the hydrogen atom, with only one electron, one proton, and no neutron. The next heavier atom, the noble gas helium, consists of two electrons, two protons, and two neutrons.

According to the Bohr model of the atom the electrons are assigned to so-called shells, which represent different energy levels and therefore are arranged concentrically around the nucleus. There is a maximum of seven shells, which can hold a different number of electrons, the electrons assignet to the outermost shell are known as valence electrons.

Simplified illustration of a neon atom

Neon atom

The efforts of all the atoms is to fulfill their outermost shell, with eight electrons they reach the so-called noble gas configuration (also electron octet). Elements with few outer electrons can donate electrons, elements with many outer electrons can accept additional valence electrons (see chapter chemical bonds for details).

Properties of atoms

Mass: The mass of an atom is determined mainly from the nucleus, since the masses of protons and neutrons (1.67·10-27 kg) are about 1,800 times larger than the mass of the electrons in the atomic shell (9.11·10-31 kg).

Dimensions: The diameter of the atomic shell is 0.1 to 0.5 nm, the diameter of the nucleus is even lower by a factor of 100,000.

To illustrate: when a pinhead in the middle of a soccer field represents the atomic nucleus, the distance to the corner flags corresponds to the distance at which the electrons orbiting the nucleus.

Density: In the nucleus of an atom, protons and neutrons are packed extremely densely. If one were to compress the earth to the same density, its radius would be reduce from 6,700,000 m initially to only 100 meters.

Elementary particles

Elementary particles

Atoms, which are important in semiconductor manufacturing

Important atoms in semiconductor industry

The elements, the periodic table

The elements

An element consists of several identical atoms and is a substance that can not be further decomposed by chemical means. The mass of elements is determined only by the number of protons and neutrons, since the electron mass is negligible. Hydrogen with one proton and no neutron has the mass number 1, the next heavier element, helium, has the mass number 4 (2 protons + 2 neutrons).

The elements are usually named with the initials of their Latin or Greek names (from latin hydrogenium: hydrogen H, from greek lithos: lithium Li).

The periodic table of the chemical elements

The periodic table of the chemical elements (periodic table) lists all the chemical elements with increasing proton number (atomic number) and according to their chemical properties, divided into periods as well as main and subgroups.

The period represents the number of electron shells, the main group, the number of electrons in the outermost shell (1 to 8 electrons). Group 1 and 2 and 13-18 are the maingroups, the group of 3-12 the subgroups.

The first element with one shell (period 1) and one outer electron (group 1) is hydrogen H. The next element, helium He, has only one electron shell and is therefore in period 1 as well. Since the first shell is completely filled with only two electrons, helium is not in group 2, but in group 18 (group of the noble gases).

To add more electrons, one needs to begin a new electron shell. Thus we find lithium Li in group 1, period 2 (two electrons on the first shell, one valence electron on the second shell). A shell can hold a maximum of 2n2 electrons, where n stands for the period.

From the fourth period there exist the groups (3-12) of the transition elements. After the first two valence electrons were added in maingroup 1 and 2 to the outermost shell, more inner shells are filled in the transitional groups for energetic reasons, before the outer shell is completely filled with electrons in maingroup 13-18.

The periodic table of the elements

  Hauptgruppen Nebengruppen Hauptgruppen
1 2 3 4 5 6 7 8 9 10 11 12 13 14 15 16 17 18
   
P
e
r
i
o
d
e
1 HElement 1: Wasserstoff (H), Nichtmetall HeElement 2: Helium (He), Edelgas
2 LiElement 3: Lithium (Li), Alkalimetall BeElement 4: Beryllium (Be), Erdalkalimetall BElement 5: Bor (B), Halbmetall CElement 6: Kohlenstoff (C), Nichtmetall NElement 7: Stickstoff (N), Nichtmetall OElement 8: Sauerstoff (O), Nichtmetall FElement 9: Fluor (F), Halogen NeElement 10: Neon (Ne), Edelgas
3 NaElement 11: Natrium (Na), Alkalimetall MgElement 12: Magnesium (Mg), Erdalkalimetall AlElement 13: Aluminium (Al), Metall SiElement 14: Silicium (Si), Halbmetall PElement 15: Phosphor (P), Nichtmetall SElement 16: Schwefel (S), Nichtmetall ClElement 17: Chlor (Cl), Halogen ArElement 18: Argon (Ar), Edelgas
4 KElement 19: Kalium (K), Alkalimetall CaElement 20: Calcium (Ca), Erdalkalimetall ScElement 21: Scandium (Sc), Übergangsmetall TiElement 22: Titan (Ti), Übergangsmetall VElement 23: Vanadium (V), Übergangsmetall CrElement 24: Chrom (Cr), Übergangsmetall MnElement 25: Mangan (Mn), Übergangsmetall FeElement 26: Eisen (Fe), Übergangsmetall CoElement 27: Cobalt (Co), Übergangsmetall NiElement 28: Nickel (Ni), Übergangsmetall CuElement 29: Kupfer (Cu), Übergangsmetall ZnElement 30: Zink (Zn), Übergangsmetall GaElement 31: Gallium (Ga), Metall GeElement 32: Germanium (Ge), Halbmetall AsElement 33: Arsen (As), Halbmetall SeElement 34: Selen (Se), Nichtmetall BrElement 35: Brom (Br), Halogen KrElement 36: Krypton (Kr), Edelgas
5 RbElement 37: Rubidium (Rb), Alkalimetall SrElement 38: Strontium (Sr), Erdalkalimetall YElement 39: Yttrium (Y), Übergangsmetall ZrElement 40: Zirkonium (Zr), Übergangsmetall NbElement 41: Niob (Nb), Übergangsmetall MoElement 42: Molybdän (Mo), Übergangsmetall TcElement 43: Technitium (Tc), Übergangsmetall RuElement 44: Ruthenium (Ru), Übergangsmetall RhElement 45: Rhodium (Rh), Übergangsmetall PdElement 46: Palladium (Pd), Übergangsmetall AgElement 47: Silber (Ag), Übergangsmetall CdElement 48: Cadmium (Cd), Übergangsmetall InElement 49: Indium (In), Metall SnElement 50: Zinn (Sn), Metall SbElement 51: Antimon (Sb), Halbmetall TeElement 52: Tellur (Te), Halbmetall IElement 53: Iod (I), Halogen XeElement 54: Xenon (Xe), Edelgas
6 CsElement 55: Cäsium (Cs), Alkalimetall BaElement 56: Barium (Ba), Erdalkalimetall LaElement 57: Lanthan (La), Übergangsmetall HfElement 72: Hafnium (Hf), Übergangsmetall TaElement 73: Tantal (Ta), Übergangsmetall WElement 74: Wolfram (W), Übergangsmetall ReElement 75: Rhenium (Re), Übergangsmetall OsElement 76: Osmium (Os), Übergangsmetall IrElement 77: Iridium (Ir), Übergangsmetall PtElement 78: Platin (Pt), Übergangsmetall AuElement 79: Gold (Au), Übergangsmetall HgElement 80: Quecksilber (Hg), Übergangsmetall TlElement 81: Thallium (Tl), Metall PbElement 82: Blei (Pb), Metall BiElement 83: Bismuth (Bi), Metall PoElement 84: Polonium (Po), Halbmetall AtElement 85: Astat (At), Halogen RnElement 86: Radon (Rn), Edelgas
7 FrElement 87: Francium (Fr), Alkalimetall RaElement 88: Radium (Ra), Erdalkalimetall AcElement 89: Actinium (Ac), Übergangsmetall RfElement 104: Rutherfordium (Rf), Übergangsmetall DbElement 105: Dubnium (Db), Übergangsmetall SgElement 106: Seaborgium (Sg), Übergangsmetall BhElement 107: Bohrium (Bh), Übergangsmetall HsElement 108: Hassium (Hs), Übergangsmetall MtElement 109: Meitnerium (Mt), Übergangsmetall DsElement 110: Darmstadtium (Ds), Übergangsmetall RgElement 111: Roentgenium (Rg), Übergangsmetall UubElement 112: Ununbium (Uub), Übergangsmetall UutElement 113: Ununtrium (Uut), Metall UuqElement 114: Ununquadium (Uuq), Metall UupElement 115: Ununpentium (Uup), Metall UuhElement 116: Ununhexium (Uuh), Metall UusElement 117: Ununseptium (Uus), UuoElement 118: Ununoctium (Uuo), Edelgas
 
CeElement 58: Cer (Ce), Lanthanoid PrElement 59: Praseodym (Pr), Lanthanoid NdElement 60: Neodym (Nd), Lanthanoid PmElement 61: Promethium (Pm), Lanthanoid SmElement 62: Samarium (Sm), Lanthanoid EuElement 63: Europium (Eu), Lanthanoid GdElement 64: Gadolinium (Gd), Lanthanoid TbElement 65: Terbium (Tb), Lanthanoid DyElement 66: Dysprosium (Dy), Lanthanoid HoElement 67: Holmium (Ho), Lanthanoid ErElement 68: Erbium (Er), Lanthanoid TmElement 69: Thulium (Tm), Lanthanoid YbElement 70: Ytterbium (Yb), Lanthanoid LuElement 71: Lutetium (Lu), Lanthanoid
ThElement 90: Thorium (Th), Actinoid PaElement 91: Protactinium (Pa), Actinoid UElement 92: Uran (U), Actinoid NpElement 93: Neptunium (Np), Actinoid PuElement 94: Plutonium (Pu), Actinoid AmElement 95: Americium (Am), Actinoid CmElement 96: Curium (Cm), Actinoid BkElement 97: Berkelium (Bk), Actinoid CfElement 98: Californium (Cf), Actinoid EsElement 99: Einsteinium (Es), Actinoid FmElement 100: Fermium (Fm), Actinoid MdElement 101: Mendelevium (Md), Actinoid NoElement 102: Nobelium (No), Actinoid LrElement 103: Lawrencium (Lr), Actinoid
 
 
Alkalimetalle Metalle Halogene Lanthanoide
Erdalkalimetalle Halbmetalle Edelgase Actinoide
Übergangsmetalle Nichtmetalle

Important elements in the semiconductor industry

Element Particle Characteristics, application
B: Boron 5p, 6n, 5e 3 valence electrons: used for p-doping of silicon
N: Nitrogen 7p, 7n, 7e Stable N2 molecule: inert gas, cover layer on top of the wafer
O: Oxygen 8p, 8n, 8e Very reactive: oxidation of silicon, insulating layers (SiO2)
F: Fluorine 9p, 10n, 9e Most reactive element: used for etching in combination with other elements (ie HF, CF4)
Si: Silicon 14p, 14n, 14e Bulk material in semiconductor industry
P: Phosphorus 15p, 16n, 15e 5 valence electrons: used for n-doping of silicon

Elements that occur on the left side in the periodic table are metals. These elements have an aspiration to donate valence electrons to achieve the noble gas configuration. On the right side there are the nonmetals, which are trying to accept additional electrons to achieve the noble gas configuration. In between there are the semimetals such as silicon and germanium.

Chemical bonds

Chemical bonds

Electrons located on the outermost shell, can escape from their atoms by supplying energy (e.g. in the form of heat) and be exchanged with other atoms. Compounds of several atoms are called molecules. The reason for the bond effort is the so-called noble gas configuration - a fulfilled valence shell - which represents an energetically stable state. Substances which have reached a full outer shell, will not form bonds (a few exceptions such as xenon-fluorine compounds are possible).

There are mainly three different types of bonds, which are discussed below.

The atomic bond

Nonmetals form this bond to achieve an octet of electrons. For example two fluorine atoms (each with seven outer electrons) can fill their octet of electrons by mutual exchange of one electron. The distance between the two nuclei represents a compromise between the attraction of the nuclei and the bonding electrons and the repulsion of the two nuclei and the electrons as well. The reason for the atomic bond is that nature is always striving to reach the lowest energy state. Since the electrons have more space through the bond of several atoms, which corresponds to a lower energy, the atomic bond is formed.

Since atoms try to achieve the fulfilled outer shell, elemental fluorine atoms never appear as a single atom, but always as a fluorine molecule F2. Similarly, nitrogen N2, oxygen O2, chlorine Cl2, bromine Br2, and Iodine I2. The atomic bond also is called covalent bond.

Illustration of the atomic bond of silane (SiH4, for silicon only the outermost shell is drawn). The silicon atom reaches the full outermost shell, the hydrogen atoms reach the filled first shell with only two electrons.

The atomic model

Atomic bond

The ionic bond

Ionic bonds are formed by the fusion of metals and nonmetals. While metals donate electrons to achieve a completely filled outer shell, nonmetals accept additional electrons. An example of an ionic bond is NaCl, sodium chloride.

The sodium atom gives off its valence electron (so it has more protons than electrons and is positively charged), while chlorine accepts one electron and thus is negatively charged. Due to the different charges the two atoms attract each other. A charged atom is known as an ion, while a positive ion is called cation and a negative ion anion, respectivley.

The ionic bond

Ionic bond
Ionic bond

Since atoms always occur at a very large number, they form grids due to the attraction and repulsion forces from ions. Substances which form such a grid in solid state, are known as salts.

Lattice of sodium chloride

ion lattice of sodium chloride

The metallic bonding

Metals are forming that bond to attain the stable noble gas configuration. Each metal atom gives off its outer electrons: thus positively charged metal ions and free electrons are genereted with strong attractive forces in between. The metal ions repel each other as well as the electrons.

Since the attraction and repulsion forces act in all dimensions of space, the atoms arrange themselves in a regular lattice. The free electrons are the so-called Fermi gas, which holds the positive metal ions together. Due to the free electrons, metal's electric conductivity is excellent.

The metallic bonding

Metallic bonding

The physical and chemical properties of compounds are dependent on the type of bonding. Thus greater attraction forces mean higher melting and boiling points, the number of free electrons affects the conductivity.

Intermolecular bondings

Intermolecular bondings differ from chemical bondings in that way that these are only forces between two ore more molucules, ions or atoms. Intermolecular bonds are caused mainly by load displacement which result in attracting or repulsing of particles.

The strongest of these forces is the hydrogen bond. Due to its bonding angle the loads inside a water molecule (H–O–H) are distributed asymmetrical, so that the oxygen atom has a negative partial charge while the hydrogen atoms have a positive partial charge. This load displacement leads to attracting and repulsing of other water molecules. Besides the hydrogen bond there are even weaker forces like the van der Waals interaction.

The bond energy of the chemical bonds is in the range of several hundreds to several thousands kilojoule/mol (kJ/mol). The bond energy of hydrogen bonds is up to a hundred kJ/mol and the bond energy of van der Waals forces is in the range of 0.5 to 5 kJ/mol.

Noble gases

Noble gases and the octet rule

Noble gases are the elements in the eighth maingroup of the periodic table: helium, neon, argon, krypton, xenon, radon (top down).

The specificity of these elements is that they have eight electrons in their outer shell. This octet represents a very stable energetic state, which all elements would like to achieve. In the chapter chemical bonds it is explaind how the elements reach a full outer shell. Due to the stable state of the noble gas configuration, these elements will not go into reaction with other elements (a few xenon-fluorine compounds and others are known).

Noble gases

Electron octet

Neon consists of ten electrons: two on the first shell and eight valence electrons on the second/outer most shell. Exception: helium, which consists of only one shell, reaches the noble gas configuration already with two electrons (electron duet instead of octet).

As inert gases [lat. inert: inactive, neutral] oxygen (eg as purge gas), argon (sputtering), and others are used in the semiconductors industry.

Conductors - Insulators - Semiconductors

Conductors

Conductors are generally substances which have the property to pass different types of energy. In the following, the conductivity of electricity is the value of interest.

Metals: The conductivity of metals is based on the free electrons (so-called Fermi gas) due to the metal bonding. Already with low energy electrons become sufficiently detached from the atoms and a conductivity is achieved.

Metallic bonding: fixed ions and free valence electrons (Fermi gas)

Metallic bonding

The conductivity depends, inter alia, on the temperature. If the temperature rises, the metal atoms swing ever stronger, so that the electrons are constrained in their movements. Consequence, the resistance increases. The best conductors, gold and silver, are used relatively rare because of the high costs (gold e.g. for the contacting of the finished chips). The alternatives in the semiconductor technology for the wiring of the individual components of microchips are aluminum and copper.

Salts: In addition to metals, salts can also conduct electricity. There are no free electrons, so the conductivity depends on ions which can be solved when a salt is melting or dissolving, so that the ions are free to move (see chapter chemical bonds for details).

Insulators

Insulators possess no free charge carriers and thus are non-conductive.

The atomic bond: The atomic bond is based on shared electron pairs of nonmetals. The elements which behave like nonmetals have the desire to catch electrons, thus there are no free electrons which might serve as charge carriers.

The ionic bond: In the solid state, ions are arranged in a grid network. By electrical forces, the particles are held together. There are no free charge carriers to enable a current flow. Thus substances composed of ions can be both conductor and insulator.

Semiconductors

Semiconductors are solids whose conductivity lies between the conductivity of conductors and insulators. Due to exchange of electrons - to achieve the noble gas configuration - semiconductors arrange as lattice structure. Unlike metals, the conductivity increases with increasing temperature.

Increasing temperatures leads to broken bonds and free electrons are generated. At the location at which the electron was placed, a so-called defect electron ("hole") remains.

Cut-out of a silicon lattice

Kein Flashplayer installiert

The electron flow is based on the conductivity properties of semiconductors. The electronic band structure illustrates why semiconductors behave like this.

The band model

The electronic band structure is an energy schema to describe the conductivity of conductors, insulators, and semiconductors. The schema consists of two energy bands (valence and conduction band) and the band gap. The valence electrons - which serve as charge carriers - are located in the valence band, in the ground state the conduction band is occupied with no electrons. Between the two energy bands there is the band gap, its width affects the conductivity of materials.

The energy bands If we consider a single atom, there are according to the Bohr model of atoms sharply distinct energy levels, which may be occupied by electrons. If there are multiple atoms side by side they are interdependent, the discrete energy levels are fanned out. In a silicon crystal, there are approximately 1023 atoms per cubic centimeter, so that the individual energy levels are no longer distinguishable from each other and thus form broad energy ranges.

Energy levels of atoms which are in interdependency with other atoms

Energy level

The width of the energy bands depends on how strongly the electrons are bound to the atom. The valence electrons in the highest energy level interact strongly with those of neighboring atoms and can be solved relatively easily from an atom; with a very large number of atoms, a single electron can no longer be assigned to one single atom. As a result, the energy bands of the individual atoms merge to a continuous band, the valence band.

Energy bands of atoms which are in interdependency with other atoms

Quantum well

The band model of conductors: In conductors, the valence band is either not fully occupied with electrons, or the filled valence band overlaps with the empty conduction band. In general, both states occure at the same time, the electrons can therefore move inside the partially filled valence band or inside the two overlapping bands. In conductors there is no band gap between the valence band and conduction band.

The band model of insulators: In insulators the valence band is fully occupied with electrons due to the covalent bonds. The electrons can not move because they're "locked up" between the atoms. To achieve a conductivity, electrons from the valence band have to move into the conduction band. This prevents the band gap, which lies in-between the valence band and conduction band.

Only with considerable energy expenditure (if at all possible) the band gap can be overcome; thus leading to a negligible conductivity.

The band model of semiconductors: Even in semiconductors, there is a band gap, but compared to insulators it is so small that even at room temperature electrons from the valence band can be lifted into the conduction band. The electrons can move freely and act as charge carriers. In addition, each electron also leaves a hole in the valence band behind, which can be filled by other electrons in the valence band. Thus one gets wandering holes in the valence band, which can be viewed as positive charge carriers.

There are always pairs of electrons and holes, so that there are as many negative as positive charges, the semiconductor crystal as a whole is neutral. A pure undoped semiconductor is known as intrinsic semiconductor. Per cubic centimeter there are about 1010 free electrons and holes (at room temperature).

Since the electrons always assume the energetically lowest state, they fall back into the valence band and recombine with the holes if there is no energy supply. At a certain temperature an equilibrium is arranged between the electrons elevated to the conduction band and the electrons falling back. With increasing temperature the number of electrons that can leap the band gap is increased, and thus increasing the conductivity of semiconductors.

The band model

Band model

Since the width of the band gap represents a certain energy corresponding to a particular wavelength, one tries to alter the width selective in order to obtain certain colors of light emitting diodes (LED). This may be achieved by combining different materials. Gallium arsenide (GaAs) has a band gap of 1.4 eV (electron volts, at room temperature) and thus emits red light.

The intrinsic conductivity of silicon is of no interest for the functioning of components, since it depends, inter alia, on the supplied energy. Which means that it changes with the temperature; in addition a conductivity comparable to metals is only possible at very high temperatures (several hundred degrees Celsius). In order to deliberately influence the conductivity of semiconductors, impurity atoms can be introduced into the regular silicon lattice to alter the number of free electrons and holes.

Doping: n- and p-semiconductors

Doping

Doping means the introduction of impurities into a semiconductor crystal to the defined modification of conductivity. Two of the most important materials silicon can be doped with, are boron (3 valence electrons = 3-valent) and phosphorus (5 valence electrons = 5-valent). Other materials are aluminum, indium (3-valent) and arsenic, antimony (5-valent).

The dopant is integrated into the lattice structure of the semiconductor crystal, the number of outer electrons define the type of doping. Elements with 3 valence electrons are used for p-type doping, 5-valued elements for n-doping. The conductivity of a deliberately contaminated silicon crystal can be increased by a factor of 106.

n-doping

The 5-valent dopant has an outer electron more than the silicon atoms. Four outer electrons combine with ever one silicon atom, while the fifth electron is free to move and serves as charge carrier. This free electron requires much less energy to be lifted from the valence band into the conduction band, than the electrons which cause the intrinsic conductivity of silicon. The dopant, which emits an electron, is known as an electron donor (donare, lat. = to give).

The dopants are positively charged by the loss of negative charge carriers and are built into the lattice, only the negative electrons can move. Doped semimetals whose conductivity is based on free (negative) electrons are n-type or n-doped. Due to the higher number of free electrons those are also named as majority charge carriers, while free mobile holes are named as the minority charge carriers.

n-doping with phosphorus

n-doping with phosphorus

Arsenic is used as an alternative to phosphorus, because its diffusion coefficient is lower. This means that the dopant diffusion during subsequent processes is less than that of phosphorus and thus the arsenic remains at the position where it was introduced into the lattice originally.

p-doping

In contrast to the free electron due to doping with phosphorus, the 3-valent dopant effect is exactly the opposite. The 3-valent dopants can catch an additional outer electron, thus leaving a hole in the valence band of silicon atoms. Therefore the electrons in the valence band become mobile. The holes move in the opposite direction to the movement of the electrons. The necessary energy to lift an electron into the energy level of indium as a dopant, is only 1 % of the energy which is needed to raise a valence electron of silicon into the conduction band.

With the inclusion of an electron, the dopant is negatively charged, such dopants are called acceptors (acceptare, lat. = to add). Again, the dopant is fixed in the crystal lattice, only the positive charges can move. Due to positive holes these semiconductors are called p-conductive or p-doped. Analog to n-doped semiconductors, the holes are the majority charge carriers, free electrons are the minority charge carriers.

p-doping with boron

p-doping with boron

Doped semiconductors are electrically neutral. The terms n- and p-type doped refer only to the majority charge carriers. Each positive or negative charge carrier belongs to a fixed negative or positive charged dopant.

N- and p-doped semiconductors behave approximately equal in relation to the current flow. With increasing amount of dopants, the number of charge carriers increases in the semiconductor crystal. Here it requires only a very small amount of dopants. Weakly doped silicon crystals contain only 1 impurity per 1,000,000,000 silicon atoms, high doped semiconductors for example contain 1 foreign atom per 1,000 silicon atoms.

Electronic band structure in doped semiconductors

Through the introduction of a dopant with five outer electrons, in n-doped semiconductors there is an electron in the crystal which is not bound and therefore can be moved with relatively little energy into the conduction band. Thus in n-doped semiconductors one finds a donator energy level near the conduction band edge, the band gap to overcome is very small.

Analog, through introduction of a 3-valent dopant in a semiconductor, a hole is available, which may be already occupied at low-energy by an electron from the valence band of the silicon. For p-doped semiconductors one finds an acceptor energy level near the valence band.

Band model of doped semiconductors

Band model of doped semiconductors

The p-n junction

p-n junction at thermal equilibrium

The p-n junction is the transition area between two n- and p-doped semiconductor crystals. In this area there are no free charge carriers, since the free electrons of the n-conductor, and the holes of the p-doped crystal in the vicinity of the interface recombine with each other, which means that the electrons fill the holes. This charge movement (diffusion) is obtained in consequence of a concentration gradient: since there is only a few number of electrons in the p-area and only a few number of holes in the n-region, the majority charge carriers (electrons in the n-crystal, holes in the p-crystal ) move into the contrary doped semiconductor. The crystal lattice at the interface must not be interrupted, a simple "pressing together" of a p-type and a n-doped silicon crystal does not allow a functional p-n junction.

The regions near the interface are loaded due to the loss of free charge carriers (positive charge in the n-crystal, negative charge in the p-crystal). The more charge carriers recombine, the greater the depletion zone and thus the voltage difference of n- and p-crystal. With a certain amount of this potential gap, the recombination of holes and electrons comes to a complete standstill, the charge carriers can no longer overcome the electric field. In silicon this limit is at about 0.7 V.

p-n junction without an external applied voltage

Kein Flashplayer installiert

A p-n junction represents an electrical component with the function to allow an electric current in one direction (called the forward biased condition) and to block the current in the opposite direction (the reverse biased condition): a diode.

p-n junction with external applied voltage

If the n-type crystal is applied to a positive and the p-crystal to a negative voltage, the electric field inside the semiconductor and the field of the voltage source are in the same direction. Thus the electric field at the p-n junction is reinforced. The oppositely charged free carriers are attracted by the poles of the voltage source, thus the barrier layer is increased and a current flow is inhibited.

If the external voltage is applied in the reverse direction, the external and internal electric field are in the opposite direction and the inner filed is weakened. If the inner field is completely eliminated from the outer field, a constantly flow of free charge carriers from the power source to the interface is possible and the carriers can recombine continuously: there is electric current.

p-n junction with an external applied voltage

Kein Flashplayer installiert

The diode can be used as a rectifier: to convert alternating current into direct current. Areas where p- and n-doped semiconductor crystals are in contact, are found in many electrical devices in the semiconductor technology.

Field-effect transistors

General layout

A transistor is an electronic semiconductor device for switching or amplifying electricity. The current can flow through two junctions - called drain and source -, while the third (gate electrode) is used for control. In addition to the field-effect transistor (FET) which is described here, there is another basic transistor, the bipolar transistor. The operation of the bipolar transistor is based on charge carriers of both polarities (thus bipolar), holes and electrons. Field-effect transistors, also known as unipolar transistors, use either electrons or holes for the transport of electricity.

The transistor is the basic component in semiconductor manufacturing, in modern microchips there are found several millions to billions of transistors. Through the combination of multiple transistors, all logic gates can be implemented in order to obtain logic output signals of corresponding input signals. Thus transistors form the heart of every microprocessor, memory chip, etc. The transistor is the most abundant object made by mankind, and thus became indispensable in today's life.

The transistor is built up layer by layer. This article describes the basic structure of a simple field-effect transistor, the various possibilities to realize the miscellaneous layers will follow in the later chapters.

Construction of a n-channel FET

1. Substrate: Basis for a n-channel field-effect transistor is a p-doped (boron) silicon substrate.

p-substrate

2. Oxidation: On top of the substrate, a thin layer of silicon dioxide SiO2 (the gate oxide) is created via thermal oxidation. It is used for insulation of the later deposited gate and the substrate.

gate oxide

3. Deposition: In a LPCVD process nitride is deposited, it is used later as an masking during the field oxidation.

Nitride deposition

4. Photolithography: On top of the nitride a photoresist is spun on, exposed and developed. Thus a structured coating layer is fabricated which serves as an etching mask.

Photolithography nitride

5. Etching: Only at resist free sites nitride is removed using reactive ion etching.

Etching of nitride

6. Resist removal: Subsequent the resist mask is removed in a wet-chemical developer solution.

Resist removal

7. Oxidation: During field oxidation, the nitride serves as a mask layer, the thermal wet oxidation takes place only on the bare gate oxide. The grown field oxide is used for lateral isolation to adjacent devices.

Field oxide

8. Etching: Subseuqent to the oxidation, the nitride is removed in a wet chemical etching process.

Nitride removal

9. Deposition: Via low pressure CVD, polycrystalline silicon is deposited which represents the gate electrode.

Gate electrode (poly silicon)

10. Photolithography: Again a resist layer on top of the polysilicon is patterned.

Photolithography gate

11. Etching: The photoresist in turn serves as a mask layer, via reactive ion etching the gate is patterned.

Gate patterning

12. Resist removal: The resist is removed via wet-chemical etching.

Resist removal

13. Oxidation: A thin oxide (post oxide) is deposited as an insulating layer for the gate electrode as well as a spacer for the subsequent source and drain implantation.

Post oxide

14. Ion implantation: Via ion implantation with phosphorus, the source and drain regions are introduced (n-type). Since the gate electrode acts as an mask during implantation, the width of the n-channel between the source and drain is preset. This is called "self alignment".

Ion implantation

15. Oxidation: As an isolation a nonmetal is deposited (e.g. oxide). This happens in a LPCVD process with TEOS, which provides a good step coverage.

Inter layer oxide

16. Photolithography and etching: In a further step a resist layer is structured and the edges of the contact holes are rounded in an isotropic etch process.

Rounding of vias

17. Etching: Subsequently the contact holes are opened in a highly anisotropic etch process.

Etching of vias

18. Metallization: The contact holes are filled with aluminum via sputtering.

Metallization (sputtering)

19. Photolithography: In a final lithography step a new resist mask is patterned.

Photolithography vias

20. Etching: The pattern is transferred into the underlying metallization in an anisotropic dry etch process.

Etching of vias

21. Resist removal: Finally, the resist is removed and aluminum conductors remain to actuate the transistor.

Resist removal

Actual the construction of a transistor is much more complex, since additional planarization layers for photolithography are neccessary or secondary drain and source implantations have to be done to adjust the threshold voltage accurately. On the slopes of the gate elektrode additional (side wall) spacers can be formed to set the exact length of the channel or fine tune the doping profile respectively.

Mode of operation

Enhancement-mode: Without a positive voltage applied to the gate there are no electrons available, which could act as free charge carriers between source and drain, since the substrate is p-doped. In steady state holes in the substrate act as majority charge carriers, while the electrons are minority charge carriers.

FET off

A positive voltage applied to the gate attracts electrons in the substrate, while holes are pushed away. Thus forming a conducting n-channel beneath the gate electrode and in-between source and drain, respectively. The insulating silicon dioxide layer prevents a current flow between the substrate and the gate.

FET on

Since the transistor blocks the current flow without an applied voltage, the transistor is also called self-locking.

Depletion-mode: With a light n-type doping between the source and drain, a conductivity is even possible without a gate voltage (a voltage between source and drain is sufficient). So-called depletion FETs, or self-conducting transistors block the current flow only, if the voltage applied to the gate electrode is lower than the voltage at the source port. If the gate voltage is decreased, the electrons that are located beneath the gate, are pushed away - the conductive electron-channel is lost.

Bipolar transistors

General layout

The second important type of transistors, next to the field-effect transistor, is the bipolar transistor. Its mode of operation is based on both charge carriers (thus bipolar), electrons and holes. Bipolar transistors are faster than field-effect transistors, however, they require more space and are therefore more expensive in mass production.

Bipolar transistors consist essentially of two mutually connected p-n junctions with the layer sequence n-p-n or p-n-p. The connections of the bipolar transistor are emitter (E), base (B) and collector (C). While emitter and collector have the same doping, the very thin base layer in-between is doped contrarily.

In this article an NPN transistor in standard buried collector (SBC) construction is described, the mode of operation of PNP transistors is analog (the signs of the applied voltages have just to be reversed).

Construction of an NPN bipolar transistor

1. Substrate: Basis for an NPN bipolar transistor is a p-doped (boron) silicon substrate, a thick oxide layer (e.g. 600 nm) is deposited on top.

p substrate

2. Buried Layer Implantation: The oxide serves as an implantation mask. As dopant antimony (Sb) is used, since its diffusion coefficient is lower than of phosphorus, and therefore the dopant won''t diffuse as much in subsequent processes. The highly n+-doped buried collector serves as a low-resistance contact surface for the collector port.

Buried layer

3. Homoepitaxy: In an epitactical process a high-impedance (low n--doped) collector layer is deposited (typically 10 microns).

Low doped homo epitaxy

4. Base implantation: With boron the p-doped base is introduced, a subsequent diffusion step magnifies its dimensions.

Base implantation

5. Emitter and collector implantation: With phosphorus both highly n+-doped emitter and collector junctions are introduced.

High doped emitter and collector

6. Metallization and photolithography: Aluminum is deposited in a sputtering process for contacting and a resist layer is patterned on top of it.

Metallization and photolithography

7. Etching: Finally, the connectors for emitter, base, and collector are structured in an anisotropic dry etch process.

Patterning of aluminum

Due to many improvements, bipolar transistor do have more than three layers (npn or pnp). Nowadays the collector region consists out of at least two variable doped zones. The terms npn and pnp just describe the active area, not the actual filmstack.

Mode of operation

The two p-n junctions are hereinafter named as EB (emitter-base) and CB (collector-base). Without an external voltage a depletion zone forms at the interfaces of EB and CB. If a negative voltage is applied to the emitter and a positive voltage is applied to the collector, the depletion zone at EB decreases, while the depletion zone at CB increases. If a positive voltage is now applied to the base, EB becomes conductive - electrons can reach the base layer. As this layer is very thin, the charge carriers can be injected into the collector, where they are extracted due to the positive external voltage. Thus, a current flow from emitter to collector is established. Almost all electrons (> 95 %) can reach the collector if only a small voltage is applied to the base, which means that with a relatively small base current (E to B) a very large collector current (E to C) is possible.

NPN transistor

The two deep p+-doped regions are used for lateral isolation from other components. In addition to the transistor a resistance (not in graphics) is needed, since bipolar transistors can not be controlled currentless.

Construction of a FinFET

General layout and mode of operation

The basic electrical layout and the mode of operation of a FinFET does not differ from a traditional field effect transistor. There is one source and one drain contact as well as a gate to control the current flow.

In contrast to planar MOSFETs the channel between source and drain is build as a three dimensional bar on top of the silicon substrate, called fin. The gate electrode is then wrapped around the channel, so that there can be formed several gate electrodes on each side which leads to reduced leakage effects and an enhanced drive current.

The manufacture of a bulk silicon-based multi gate transistor with three gates (tri gate) is described below.

Construction of a bulk silicon-based FinFET

1. Substrate: Basis for a FinFET is a lightly p-doped substrate with a hard mask on top (e.g. silicon nitride) as well as a patterned resist layer.

Substrate

2. Fin etch: The fins are formed in a highly anisotropic etch process. Since there is no stop layer on a bulk wafer as it is in SOI, the etch process has to be time based. In a 22 nm process the width of the fins might be 10 to 15 nm, the height would ideally be twice that or more.

Fin etch

3. Oxide deposition: To isolate the fins from each other a oxide deposition with a high aspect ratio filling behavior is needed.

Oxide deposition

4. Planarization: The oxide is planarized by chemical mechanical polishing. The hard mask acts as a stop layer.

Planarization

5. Recess etch: Another etch process is needed to recess the oxide film to form a lateral isolation of the fins.

Recess etch

6. Gate oxide: On top of the fins the gate oxide is deposited via thermal oxidation to isolate the channel from the gate elctrode. Since the fins are still connected underneath the oxide, a high-dose angled implant at the base of the fin creates a dopant junction and completes the isolation (not illstrated).

Gate oxide

7. Deposition of the gate: Finally a highly n+-doped poly silicon layer is deposited on top of the fins, thus up to three gates are wrapped around the channel: one on each side of the fin, and - depending on the thickness of the gate oxide on top - a third gate above.

Gate electrode

The influence of the top gate can also be inhibited by the deposition of a nitride layer on top of the channel.

Since there is an oxide layer on an SOI wafer, the channels are isolated from each other anyway. In addition the etch process of the fins is simplified as the process can be stopped on the oxide easily.

SOI-based FinFET



Semiconductor Technology from A to Z: Fundamentals