Virtual Twins and Machine Learning Raise DRAM Yield in a Calibrated Process Model

November 19, 2026

Virtual Twins and Machine Learning Raise DRAM Yield in a Calibrated Process Model

Image: ChatGPT

As DRAM1. dynamic random access memoryMemory technology or system for temporarily or permanently storing digital information.2. dynamic random-access memoryDRAM is a volatile memory technology manufacturing scales further, process flows are becoming more complex, process windows are tightening, and new sources of variation are making acceptable yield harder to reach. A major concern is the rise of systemic failures during yield ramp, where multiple process modules interact and create correlated defects rather than isolated random events.

To address that problem, process engineers combined a calibrated virtual twin with machine-learning optimization. The approach uses a virtual manufacturing model, SEMulator3D, together with Fabtex Yield Optimizer to predict process failures and explore process changes in a digital environment before committing to wafer-based trials.

The virtual twin reproduces process variation in a calibrated setting and supports yield analysis by evaluating several failure mechanisms at once. Machine learning then compares alternative process changes and structural variations simultaneously, reducing the need for extensive silicon experimentation while still allowing engineers to test a broad solution space.

In the case study, a DRAM1. dynamic random access memoryMemory technology or system for temporarily or permanently storing digital information.2. dynamic random-access memoryDRAM is a volatile memory technology manufacturing sequence was modeled with virtual metrology measurements inserted throughout the process flow. The model was calibrated against silicon data so that the simulated behavior more closely matched observed manufacturing results and could serve as the basis for failure analysis and optimization.

The calibrated model contained eight known systemic failure mechanisms. These included shorts, opens, and overlap-related defects affecting critical DRAM1. dynamic random access memoryMemory technology or system for temporarily or permanently storing digital information.2. dynamic random-access memoryDRAM is a volatile memory technology structures. Each failure mode was translated into a measurable geometric condition, allowing virtual metrology to detect and analyze multiple defects automatically within a single study.

Machine learning was then used to optimize process targets across all eight predefined failure modes at the same time. Instead of tuning each defect mechanism separately, the optimization searched for process settings that reduced the overall failure rate and improved the pass ratio across the full set of systemic issues.

The results were substantial. Under nominal process conditions, the predicted total yield was 0.1 %. After optimization, the predicted yield increased to 78.5 %, with lower failure rates across all eight mechanisms. The optimized solution was also translated into actionable inline fab targets that can be applied to the real process to guide further adjustments in process and structural parameters.

The workflow shows how calibrated process models and machine learning can speed up DRAM1. dynamic random access memoryMemory technology or system for temporarily or permanently storing digital information.2. dynamic random-access memoryDRAM is a volatile memory technology yield improvement by identifying multiple failure modes in parallel and narrowing the search for effective process corrections without extensive wafer experimentation.

Source: Semiconductor Engineering