Qnity is entering its second year as a standalone electronics materials company with a sharper focus on the semiconductor supply chain. After the separation from DuPont was completed on Nov. 1, 2025, the company says it has reorganized itself to operate at the pace required by chipmakers, where materials must be qualified years before volume production and delays can affect entire roadmaps.
The portfolio spans CMP1. chemical mechanical planarizationFlattening of wafer surfaces through combined chemical and mechanical material removal.2. chemical mechanical polishingWafer planarization combining chemical reactions with mechanical material removal. materials, lithography materials, specialty cleans, selective etchants, high-performance seals, electrodeposited metallization, dry-film photoresists, dielectrics and flexible laminates. Qnity also supplies EMIelectromagnetic interferenceUnwanted electromagnetic disturbance affecting electronic devices. shielding and thermal management materials aimed at preserving signal integrity, limiting interference and handling rising heat loads in advanced electronic systems.
At the center of the current technology shift is what Qnity describes as a move from shrink to shrink and stack. As transistor scaling reaches single-digit nanometer dimensions, the industry is relying more heavily on gate-all-around structures, 3D NAND1. Not ANDA logic gate that outputs 0 when all inputs are 1, and outputs 1 in all other cases2. negative-ANDNAND denotes a logic operation and is also the name of a widely used flash memory type. with 300 to 400 layers and heterogeneous integration through advanced packaging. Memory and logic are increasingly placed side by side in 2.5D designs or stacked directly in 3D packages.
That transition is making materials problems more visible. Hybrid bonding can improve energy efficiency and signal transfer, but it demands extremely precise alignment, new copper polishing approaches and materials that can support tighter integration. As package density rises, planarization has to handle combinations of inorganic and organic materials, which creates new requirements for pads, slurries and cleans.
Mechanical stress is also becoming a limiting factor. Differences in coefficients of thermal expansion between layers can lead to warpage, and severe warpage can trigger reliability issues. Qnity says those effects are pushing advanced materials higher up the design stack as packaging architectures become more complex.
AIartificial intelligenceAI stands for artificial intelligence workloads are amplifying the pressure on the package and on the board. The company points to shorter copper interconnects, backside power delivery and co-packaged optics as approaches that can reduce energy consumption and wasted heat. Optical links are gaining attention because they can move more compute capability with less heat than electrical wiring.
Qnity is also using AIartificial intelligenceAI stands for artificial intelligence in its own materials development flow. The company says computational modeling and agentic AIartificial intelligenceAI stands for artificial intelligence are helping accelerate discovery and qualification, and in some cases development timelines have been cut by 30 %. The goal is to get materials working not only in the lab, but on customer equipment and in customer process flows, where the next node is already being prepared years in advance.